Application
These consumables are designed to match alloys commonly used in castings. The addition of copper not only improves corrosion resistance in sulfuric acid environments but also has the potential to enhance strength and wear resistance. It's important to highlight that, compared to alloys with less than 1% copper, the as-welded toughness and resistance to pitting in chloride environments may be reduced. The composition is carefully controlled to maintain a minimum Pitting Resistance Equivalent (PRE) of 40, aligning with superduplex alloys for optimal pitting resistance. However, for applications in non-sulfuric acid media, consumables with less than 1% copper may be preferred, unless post-weld heat treatment (PWHT) is applied. These consumables find applications in pumps, valves, corrosion-resistant and wear-resistant components, as well as process equipment suitable for use in offshore oil and gas industries, pulp and paper, textile industries, and chemical and petrochemical plants.
Alloy Type
Austenitic heat resisting consumables to match alloy 800.
Microstructure
As-welded weld metal microstructure consists of austenite with cellular NbC-rich network.
Materials

EN W.Nr.: 1.4850, 1.4859, 1.4876.
ASTM: A351 CT15C.
UNS: N08800, N08810, N08811.
PROPRIETARY: Paralloy CR32W (Doncasters Paralloy), Incoloy® 800, 800H, 800HT (Special Metals), Manaurite® 900 (Manoir Industries), Thermalloy T52 (Lloyds), Sanicro 31 (Sandvik), Vicro 8 (Firth Vickers), RA330 (Rolled Alloys), MO-RE® 21 (Duraloy), Nicrofer 3220 (VDM), Centralloy® 4859 (Schmidt + Clemens), E2032Nb (Engemasa).
Welding & PWHT
No preheating is deemed necessary, and it is preferable to maintain the interpass temperature below 150°C. Ordinarily, welds do not undergo heat treatment. However, in applications involving elevated temperatures, the Heat-Affected Zone (HAZ) of welds in alloys 800/800H/800HT, characterized by progressively increasing levels of Ti+Al, may exhibit susceptibility to stress relaxation cracking. For pressure boundary welds designed to operate at temperatures exceeding 538°C, compliance with ASME VIII UNF-56 is mandated. This standard stipulates a Post-Weld Heat Treatment (PWHT) requirement at temperatures surpassing 885°C for 1 hour, with an additional hour for every 25mm (e.g., 900°C for 3 hours), or alternatively, the application of solution annealing. Notably, API 560 does not currently enforce a PWHT requirement. However, it's essential to acknowledge that certain specifiers may insist on PWHT for specific operating conditions.

Products of the line 800/800H

Product name Process AWS specifications EN ISO specifications
DAIKOWT 21.33MnNb GTAW - -
G-TECH 800Nb SMAW -
EN ISO 3581-A
EZ 21 32 MnNb B 32
DAIKOWM 21.33MnNb GMAW - -
DAIKOWS 21.33MnNb SAW - -

DO YOU NEED HELP?

Go to our dedicated section or contact us
Daiko supporting the environment
Questo sito si avvale di cookie necessari al suo funzionamento ed utili alle finalità illustrate nella cookie policy.

Carrello

Il carrello è vuoto