DAIKOMCW 115

FCAW
  • HIGH YIELD STRENGTH STEELS
110ksi

Description

Metal all position flux cored wire
Virtually spatter free in the spray-arc range and particularly suitable for robotic applications, this Ni-Cr-Mo low alloy metal core wire is formulated for welding high yield strength steels, with tensile strength higher than 770 MPa. Excellent resilience values ​​at low temperatures, down to -60°C. Suitable for carpentry, off-shore constructions, chemical and petroleum industries. It can be used in the construction of industrial machines, cranes, and other components that require high mechanical strength.
Specifications
EN ISO 18276-A
69 6 Mn2NiCrMo M M21 H5
AWS A5.36
E111T1-15
Shielding
M21
Positions
PA, PB, PC, PD, PE, PF, PG
Current
DC+
Packaging Type
BS300 spool
Asme qualifications
F-No (QW432)
6
A-No (QW442)
10
Chem. Comp. %
DEFAULT
C
0.07
Mn
1.4
Ni
2.2
Cr
0.35
P
0.02
S
0.02
Mo
0.4
Si
0.4
Cu
0.15
Mechanical Properties
min
variant
Tensile strength Rm MPa
760
900
Yield strength Rp0.2 MPa
690
690
Elongation A (L0=5d0) %
17
17
Impact Charpy ISO-V
47J @ -60°C
47J @ -60°C
Impact Charpy ISO-V
-
-
Welding Parameters
1.2 mm
1.6 mm
Ampere
160A - 280A
180A - 350A
Voltage
18V - 30V
30V - 34V
Packaging
Ø 1,2÷1,6mm
Ø 1,2÷1,6mm
Packaging Type
product.packaging_types.product.packaging_types.product.packaging_types.BS300 spool
product.packaging_types.product.packaging_types.product.packaging_types.BS300 spool
Description

Application

Ideal for joining high-strength thermomechanically refined and quenched and tempered fine-grain structural steels and tubes. The deposited metal provides excellent strength even at low temperatures when used with gas mixes. It has good deformability, making it particularly suitable for use in crane construction, buildings, and vehicles. It is critical to preheat according to base material and thickness; materials that could be welded with higher-strength consumables normally require a minimum preheat of 100 °C. For some HSLA steels, exceeding interpass temperatures of 200 °C can compromise strength and toughness. The post-weld heat treatment (PWHT) varies depending on the base material and the specified application.

Alloy Type

Mn-Ni-Mo low alloy consumables for welding high strength steels with ultimate tensile strength up to 750 MPa (110 ksi).

Microstructure

The microstructure of all the consumables is predominantly ferrite; some will contain high proportions of acicular ferrite for optimum as-welded toughness

Materials

For joining of quenched and tempered and thermomechanically rolled fine-grained structural steels. For use in building, crane and vehicle constructions.
  • EN W.Nr.: S690QL1, L555M, S690Q, S690QL, S690QL1, S650MC, S700MC
  • ASTM: A 514 Gr. F, H, Q
  • API: 5L X80, 5L X90, 5L X100
  • PROPRIETARY: N-A-XTRA® M 700 (ThyssenKrupp), Strenx® 700 (SSAB)

DO YOU NEED HELP?

Go to our dedicated section or contact us
DAIKO supporting the environment
Questo sito si avvale di cookie necessari al suo funzionamento ed utili alle finalità illustrate nella cookie policy.

Carrello

Il carrello è vuoto