DAIKOWS 347

SAW
  • AUSTENITIC STAINLESS STEELS
347

Description

Solid wire for stabilised austenitic stainless steels
These Cr-Ni consumables are Nb-stabilized for welding steels grades, such as 321 and 347, that are stabilized with Ti or Nb. The presence of Nb reduces intergranular corrosion under severe operation conditions. Also suitable for cladding as on mild steel after a 309 buffer layer. Service temperatures are typically -100°C to about 400°C. If dilution by the base metal produces a low ferrite or fully austenitic weld metal, the crack sensitivity of the weld may increases substantially.
Specifications
ISO 14343-A
S 19 9 Nb
AWS A5.9
ER347
Certifications
CE
Shielding
DAIKOFLUX 900-W
Positions
PA, PB, PC
Current
DC/AC
Packaging Type
K415 spool and drums.
Asme qualifications
F-No (QW432)
6
A-No (QW442)
8

Ferrite

3-12 FN

Pren

19.165

Hardness

84HRB
Chem. Comp. %
DEFAULT
C
0.05
Mn
0.7
Ni
10
Cr
19
Nb
0.4
P
0.02
S
0.01
Mo
0.05
Si
0.9
Cu
0.07
Mechanical Properties
min
variant
Tensile strength Rm MPa
550
570
Yield strength Rp0.2 MPa
350
360
Elongation A (L0=5d0) %
25
30
Impact Charpy ISO-V
-
80J @ 20°C
Impact Charpy ISO-V
-
-
Welding Parameters
2.4 mm
Ampere
300A - 400A
Voltage
27V - 33V
Packaging
Ø 2,0÷4,0mm
Packaging Type
K415 spool and drums.
347
Description

Application

Developed for welding Ti and Nb-stabilized 18Cr/8Ni stainless steel types 321 and 347, they are also suitable for unstabilized grades like 304/304L. Service temperatures typically range from -100°C to about 400°C. The applications parallel those of 308L, covering diverse sectors such as food, brewery, pharmaceutical equipment, architectural and general fabrication, and nuclear engineering. However, the 347 consumables mentioned here are generally unfit for elevated temperature structural applications where 0.04-0.08% carbon is specified for creep resistance; for such cases, consult data sheets 347H. For cryogenic uses requiring >0.38mm (15mils) Charpy lateral expansion at –196°C, select unstabilized weld metal with low carbon and controlled ferrite. No preheating requirement, a recommended maximum interpass temperature of 250°C, and no post-weld heat treatment (PWHT) necessity.

Alloy Type

347 austenitic stainless steel for joining 321 and 347 base materials.

Microstructure

Austenite with a controlled level of ferrite, normally in the range 3-12FN.

Materials


EN W.Nr.: 1.4541, 1.4543, 1.4561, 1.4550, 1.4552 (cast).
ASTM: 321, 347, CF8C (cast).
UNS: S32100, S34700.

DO YOU NEED HELP?

Go to our dedicated section or contact us
Daiko supporting the environment
Questo sito si avvale di cookie necessari al suo funzionamento ed utili alle finalità illustrate nella cookie policy.

Carrello

Il carrello è vuoto